NUCLEI GU IN FERRITE


|
MODELLO |
G.W |
DIMENSIONE(mm) |
||||||
|
A |
B |
C |
D |
E |
F |
G |
||
|
GU14/9 |
5 |
14.2±0.25 |
11.95±0.2 |
5.85±0.2 |
\ |
2.9±0.1 |
4.45±0.1 |
3.8±0.6 |
|
GU26/16 |
26 |
25.5±0.5 |
21.5±0.3 |
11.3±0.2 |
5.5±0.15 |
5.6±0.1 |
8.0±0.1 |
3.8±0.6 |
|
GU30/19 |
40 |
30.0±0.5 |
25.4±0.4 |
13.3±0.2 |
5.5±0.15 |
6.6±0.1 |
9.45±0.1 |
4.3±0.6 |
|
GU36/22 |
67 |
35.6±0.6 |
30.4±0.5 |
15.9±0.3 |
5.5±0.15 |
7.4±0.1 |
11.0±0.1 |
4.4±0.6 |
|
GU48/30 |
148 |
47.5±0.5 |
40,8 minuti |
19.2±0.4 |
5.8±0.2 |
10.6±0.3 |
14.8±0.3 |
8.4±0.6 |
|
GU50 |
178 |
50.0±0.5 |
44.0±0.5 |
16.0±0.3 |
\ |
17.0±0.3 |
20.0±0.3 |
6.2±0.6 |
|
MODELLO |
PARAMETRO |
AL±25%(nH/N^2) |
N.W(g) |
|||||
|
C1mm-1 |
Lemm |
Ehm2 |
Vemm3 |
ZP40 |
||||
|
GU14/9 |
0.790 |
19.8 |
25.1 |
495 |
2000 |
4.5 |
||
|
GU26/16 |
0.400 |
37.6 |
93.9 |
3530 |
4600 |
20.0 |
||
|
GU30/19 |
0.330 |
45.2 |
137.0 |
6190 |
5700 |
34.0 |
||
|
GU36/22 |
0.260 |
53.2 |
202.0 |
10700 |
7300 |
60.0 |
||
|
GU48/30 |
0.230 |
72.7 |
313.4 |
22780 |
7300 |
134.0 |
||
|
GU50 |
0.43 |
96.9 |
226.0 |
21900.0 |
5000 |
160 |
||