NUCLEI IN FERRITE EFD

NUCLEI IN FERRITE EFD

product-705-272

 

MODELLO

G.W

DIMENSIONE(mm)

A

B

C

D

C

F

G

H

EFD20

9

20.0±0.6

15.4±0.5

8.9±0.2

6.7±0.2

7.7±0.3

10.0±0.3

0.2±0.1

3.6±0.2

EFD21A

9

20.8±0.6

15,4 minuti

8.9±0.2

6.7±0.2

7.7±0.3

10.0±0.3

0.2±0.1

3.6±0.2

EFD21B

9.7

21.0±0.5

15,4 minuti

8.9±0.2

6.7±0.2

8.0±0.3

10.3±0.3

\

3.6±0.2

EFD25.6

19

25.6±0.7

19.5±0.7

11.4±0.3

9.1±0.3

9.3±0.3

12.5±0.3

0.6±0.1

5.2±0.3

EFD31

25

30.8±0.8

23,2 minuti

14.4±0.3

8.8±0.2

11.2±0.3

15.0±0.3

0.3±0.2

4.8±0.2

EFD34

29.6

34.0±0.6

24.0±0.5

17.0±0.3

5.0±0.2

18.0±0.3

23.0±0.3

\

3.0±0.2

EFD40/45/11

60

40.5±0.7

30.0min

16.6±0.3

10.6±0.2

16.3±0.3

22.5±0.3

\

6.6±0.2

EFD40/44/8

44

40.0±0.7

29,5 minuti

19.9±0.4

8.0±0.2

17.1±0.3

22.0±0.3

\

4.0±0.2

EFD43/53/4.4

63.6

43.0±0.8

28,5 minuti

21.6±0.4

7.6±0.25

19.3±0.3

26.5±0.3

\

4.4±0.25

EFD43/44/3.2

49.2

43.4±0.8

33,5 minuti

22.3±0.4

8.0±0.25

17.1±0.3

22.2±0.3

\

3.2±0.25

EFD45/50

67

45.2±0.8

33.3±0.8

24.0±0.4

7.8±0.2

18.0±0.3

24.7±0.3

\

4.0±0.2

EFD52.5

118

52.5±1.1

39 minuti

22.5±0.4

13.0±0.3

19.9±0.3

27.0±0.3

\

7.5±0.3

 

MODELLO

PARAMETRO

AL±25%(nH/N^2)

N.W(g)

C1mm-1

Lemm

Ehm2

Vemm3

ZP40

EFD20

1.52

47.0

31.0

1460.0

1150

7.9

EFD21A

1.57

49.3

31.0

1460.0

1400

7.9

EFD21B

1.57

49.3

31.4

1540.0

1450

8.6

EFD25.6

1.00

57.0

58.0

3300.0

2000

16.5

EFD31

0.99

68.2

69.1

4712.0

2000

23.0

EFD34

1.90

95.0

50.0

4750.0

1400

33.5

EFD40/45/11

1.02

108.8

106.5

10951.0

2300

55.0

EFD40/44/8

1.35

102.8

75.5

7750.0

1700

38.0

EFD43/53/4.4

1.14

111.3

99.8

11113.0

2000

59.0

EFD43/44/3.2

1.41

102.0

72.1

7352.0

1500

43.0

EFD45/49

1.08

108.0

97.7

10356.2

2700

60.0

EFD52.5

0.78

132.0

168.0

23250.0

2750

109.0